J 2022

Aluminum Melt Degassing Process Evaluation Depending on the Design and the Degree of the FDU Unit Graphite Rotor Wear

PODAŘIL, Martin; Ján MAJERNÍK; Rudolf KAMPF; Ladislav SOCHA; Karel GRYC et al.

Základní údaje

Originální název

Aluminum Melt Degassing Process Evaluation Depending on the Design and the Degree of the FDU Unit Graphite Rotor Wear

Autoři

PODAŘIL, Martin; Ján MAJERNÍK; Rudolf KAMPF; Ladislav SOCHA; Karel GRYC; Tomáš PRÁŠIL a Martin GRÁF

Vydání

Materials, Switzerland, MDPI, 2022, 1996-1944

Další údaje

Jazyk

angličtina

Typ výsledku

Článek v odborném periodiku

Obor

20301 Mechanical engineering

Stát vydavatele

Švýcarsko

Utajení

není předmětem státního či obchodního tajemství

Odkazy

Impakt faktor

Impact factor: 3.400

Označené pro přenos do RIV

Ano

Kód RIV

RIV/75081431:_____/22:00002297

Organizační jednotka

Vysoká škola technická a ekonomická v Českých Budějovicích

EID Scopus

Klíčová slova anglicky

aluminum alloys; refining; melt degassing; FDU unit; graphite rotor

Štítky

Návaznosti

TH04010449, projekt VaV.
Změněno: 21. 3. 2023 18:31, Mgr. Nikola Petříková

Anotace

V originále

One of the most important indicators of casting quality is porosity. The formation of pores is largely conditioned by the presence of hydrogen in the batch and subsequently in the melt. The gasification of the melt is the primary factor increasing the porosity of casts. This paper addresses the issue of reducing the melt gasification by using FDU (Foundry Degassing Unit) unit. The gas content in the melt is evaluated by determining the Dichte Index depending on the geometry and the degree of the FDU unit rotor wear. For experiments performed under the operating conditions, three types of graphite rotors with different geometries are used. The extent of melt gasification and the Dichte Index are monitored during the rotor wear, at a rate of 0%, 25%, 50%, 75% and 100% rotor wear. Secondly, the chemical composition of the melt is monitored depending on the design and wear of the rotor. It is proven that the design and the degree of rotor wear do not have significant effect on the chemical composition of the melt and all evaluated samples fell within the prescribed quality in accordance with EN 1706. With regard to the overall comparison of the geometry and wear of individual rotor types, it has been proven that, in terms of efficiency, the individual rotors are mutually equivalent and meet the requirements for melt degassing throughout the service life.

Přiložené soubory

materials-15-04924__1_.pdf
Požádat o autorskou verzi souboru