The Piston Velocity Impact on the Filling Chamber Wave Formation of High Pressure Die Casting Machine in 1st Phase of Casting Cycle

MAJERNÍK, Ján and Martin PODAŘIL

Basic information

Original name

The Piston Velocity Impact on the Filling Chamber Wave Formation of High Pressure Die Casting Machine in 1st Phase of Casting Cycle

Name in Czech

Vliv rychlosti pístu na tvorbu vln v plnicí komoře vysokotlakého licího stroje v 1. fázi licího cyklu

Authors

MAJERNÍK, Ján and Martin PODAŘIL

Edition

International journal of advanced manufacturing technology, London, Springer, 2023, 0268-3768

Other information

Language

English

Type of outcome

Article in a journal

Field of Study

20300 2.3 Mechanical engineering

Country of publisher

United Kingdom of Great Britain and Northern Ireland

Confidentiality degree

is not subject to a state or trade secret

References:

Impact factor

Impact factor: 2.900

Marked to be transferred to RIV

Yes

RIV identification code

RIV/75081431:_____/23:00002588

Organization unit

Institute of Technology and Business in České Budějovice

EID Scopus

Keywords (in Czech)

Plnění komory; zachycení plynu; HPDC; rychlost pístu; pórovitost

Keywords in English

Chamber Filling; Gas Entrapment; HPDC; Piston velocity; Porosity

Tags

Tags

Reviewed
Changed: 6/10/2023 10:56, Barbora Kroupová

Abstract

In the original language

The quality properties of high pressure die casts are closely correlated with porosity. The formation of porosity is primarily initiated by entrapment of air and gases in the volume of the melt, during its transition through the gating system. This entrapment can occur as a result of an incorrect design of the gating system, incorrect setting of the casting technological parameters, or sometimes a combination of both causes. The setting of the piston velocity in the first and second phase of the casting cycle has the highest proportion of the gas entrapment of all the technological parameters. The submitted article is describing the influence of piston velocity in the first phase of the casting cycle. Velocities are investigated in range from 0.1 m.s-1 to 1.3 m.s-1. First of all, the development of the wave arising at different piston velocities is assessed and the gas entrapment in the melt volume is investigated. Subsequently, the proportion of the gas entrapment in the cast volume at the end of the filling phase is investigated depending on the variable value of the piston velocity in the first phase. In the end, the determination of the piston velocity impact in the first phase on the completion nature of the filling chamber of the machine is derived.

In Czech

Kvalitativní vlastnosti vysokotlakých tlakových odlitků úzce souvisejí s pórovitostí. Vznik pórovitosti je iniciován především zachycením vzduchu a plynů v objemu taveniny při jejím průchodu vtokovým systémem. K tomuto zachycení může dojít v důsledku nesprávné konstrukce vtokového systému, nesprávného nastavení technologických parametrů odlévání nebo někdy kombinací obou příčin. Nastavení rychlosti pístu v první a druhé fázi licího cyklu má ze všech technologických parametrů nejvyšší podíl na zachycení plynu. Předkládaný článek popisuje vliv rychlosti pístu v první fázi licího cyklu. Rychlosti jsou zkoumány v rozsahu od 0,1 m.s-1 do 1,3 m.s-1. Především je posuzován vývoj vlny vznikající při různých rychlostech pístu a zkoumáno zachycení plynu v objemu taveniny. Následně se zkoumá podíl zachycení plynu v objemu odlitku na konci fáze plnění v závislosti na proměnné hodnotě rychlosti pístu v první fázi. Nakonec je odvozeno určení vlivu rychlosti pístu v první fázi na charakter plnění plnicí komory stroje.