J 2022

Impact of Rotor Material Wear on the Aluminum Refining Process

PRÁŠIL, Tomáš; Ladislav SOCHA; Karel GRYC; Jana SVIŽELOVÁ; Mariola SATERNUS et al.

Základní údaje

Originální název

Impact of Rotor Material Wear on the Aluminum Refining Process

Autoři

PRÁŠIL, Tomáš; Ladislav SOCHA; Karel GRYC; Jana SVIŽELOVÁ; Mariola SATERNUS; Tomasz MERDER; Jacek PIEPRZYCA a Martin GRÁF

Vydání

Materials, Basel, Switzerland, MDPI, 2022, 1996-1944

Další údaje

Jazyk

angličtina

Typ výsledku

Článek v odborném periodiku

Obor

20500 2.5 Materials engineering

Stát vydavatele

Švýcarsko

Utajení

není předmětem státního či obchodního tajemství

Odkazy

URL

Impakt faktor

Impact factor: 3.400

Označené pro přenos do RIV

Ano

Kód RIV

RIV/75081431:_____/22:00002311

Organizační jednotka

Vysoká škola technická a ekonomická v Českých Budějovicích

UT WoS

000825651000001

EID Scopus

2-s2.0-85134430466

Klíčová slova anglicky

aluminum refining; graphite wear; wear testing; rotary impeller

Štítky

RIV22, WOS

Návaznosti

TH04010449, projekt VaV.
Změněno: 21. 3. 2023 13:31, Barbora Kroupová

Anotace

V originále

The paper presents the results of tests carried out during the refining of the AlSi9Cu3(Fe) alloy in industrial conditions at the FDU stand. In the tests, three different rotors made of classical graphite, fine-grained graphite and classical graphite with SiC spraying were tested for the degree of wear. A series of tests was conducted for five cases—0% to 100% of consumption every 25%—corresponding to the cycles of the refining process. The number of cycles corresponding to 100% wear of each rotor was determined as 1112. The results of the rotor wear profile for all types of graphite after the assumed cycles are presented. Comparison of CAD models of new rotors and 3D scans of rotors in the final stage of operation revealed material losses during operational tests. The study assessed the efficiency of the rotor in terms of its service life as well as work efficiency. It was estimated on the basis of the calculated values of the Dichte Index (DI) and the density of the samples solidified in the vacuum. The structure of samples before and after refining at various stages of rotor wear is also presented, and the results are discussed.
Zobrazeno: 18. 11. 2026 21:07