2022
Impact of Rotor Material Wear on the Aluminum Refining Process
PRÁŠIL, Tomáš; Ladislav SOCHA; Karel GRYC; Jana SVIŽELOVÁ; Mariola SATERNUS et al.Základní údaje
Originální název
Impact of Rotor Material Wear on the Aluminum Refining Process
Autoři
PRÁŠIL, Tomáš; Ladislav SOCHA; Karel GRYC; Jana SVIŽELOVÁ; Mariola SATERNUS; Tomasz MERDER; Jacek PIEPRZYCA a Martin GRÁF
Vydání
Materials, Basel, Switzerland, MDPI, 2022, 1996-1944
Další údaje
Jazyk
angličtina
Typ výsledku
Článek v odborném periodiku
Obor
20500 2.5 Materials engineering
Stát vydavatele
Švýcarsko
Utajení
není předmětem státního či obchodního tajemství
Odkazy
Impakt faktor
Impact factor: 3.400
Označené pro přenos do RIV
Ano
Kód RIV
RIV/75081431:_____/22:00002311
Organizační jednotka
Vysoká škola technická a ekonomická v Českých Budějovicích
UT WoS
EID Scopus
Klíčová slova anglicky
aluminum refining; graphite wear; wear testing; rotary impeller
Návaznosti
TH04010449, projekt VaV.
Změněno: 21. 3. 2023 13:31, Barbora Kroupová
Anotace
V originále
The paper presents the results of tests carried out during the refining of the AlSi9Cu3(Fe) alloy in industrial conditions at the FDU stand. In the tests, three different rotors made of classical graphite, fine-grained graphite and classical graphite with SiC spraying were tested for the degree of wear. A series of tests was conducted for five cases—0% to 100% of consumption every 25%—corresponding to the cycles of the refining process. The number of cycles corresponding to 100% wear of each rotor was determined as 1112. The results of the rotor wear profile for all types of graphite after the assumed cycles are presented. Comparison of CAD models of new rotors and 3D scans of rotors in the final stage of operation revealed material losses during operational tests. The study assessed the efficiency of the rotor in terms of its service life as well as work efficiency. It was estimated on the basis of the calculated values of the Dichte Index (DI) and the density of the samples solidified in the vacuum. The structure of samples before and after refining at various stages of rotor wear is also presented, and the results are discussed.