2022
COMPARISON OF POROSITY OF CASTS PRODUCED BY HPDC AND VPDC TECHNOLOGIES
GAŠPÁR, Gašpár; Ján MAJERNÍK; Mirosław TUPAJ a Martin PODAŘILZákladní údaje
Originální název
COMPARISON OF POROSITY OF CASTS PRODUCED BY HPDC AND VPDC TECHNOLOGIES
Autoři
GAŠPÁR, Gašpár; Ján MAJERNÍK; Mirosław TUPAJ a Martin PODAŘIL
Vydání
MM SCIENCE JOURNAL, Prague, MM Science, PRIPOCNI 1519-10A, PRAGUE 10 10100, CZECH REPUBLIC, 2022, 1803-1269
Další údaje
Jazyk
angličtina
Typ výsledku
Článek v odborném periodiku
Obor
20301 Mechanical engineering
Stát vydavatele
Česká republika
Utajení
není předmětem státního či obchodního tajemství
Odkazy
Impakt faktor
Impact factor: 0.700
Označené pro přenos do RIV
Ano
Kód RIV
RIV/75081431:_____/22:00002282
Organizační jednotka
Vysoká škola technická a ekonomická v Českých Budějovicích
UT WoS
Klíčová slova anglicky
Vacuum Pressure Die Casting (VPDC); High Pressure Die Casting (HPDC); Porosity; Gas Entrapment; Zinc Alloys
Změněno: 4. 4. 2022 08:17, Mgr. Nikola Petříková
Anotace
V originále
The die casting technology enables the production of complex casts with good mechanical properties and high repeatability of the production within narrow tolerance limits. However, the casts are showing signs of porosity to some extent, which may reduce their mechanical and qualitative properties. The presented article solves the problem of reducing the porosity f the high pressure die casts by vacuuming the mold. Under constants technological parameters of casting, series of casts are being casted using the HPDC and VPDC technology. The indirect method of verifying the density and volume of individual samples is used to analyze the porosity of casts. At the same time, a macroscopic examination of the homogeneity of the casts is performed on selected samples. Macroscopic examination showed a detectable decrease in pore size and distribution in the casts. Based on the measurements, i tis proved that by using the vacuum pressure die casting process while maintaining the constant settings of the technological parameters of casting, a reduction in the porosity of the casts by an average of 24.4 % was achieved