2017
Issue of Changes in Adhesion of Bitumen Sheet to Primary Layer over the Course of Time in Multilayer Waterproofing during Shear Testing
PLACHÝ, Jan; Jana VYSOKÁ; Radek VEJMELKA; Jan HORSKÝ; Vítězslav VACEK et al.Basic information
Original name
Issue of Changes in Adhesion of Bitumen Sheet to Primary Layer over the Course of Time in Multilayer Waterproofing during Shear Testing
Name in Czech
Problematika změn adheze asfaltového pásu k primární vrstvě v čase v hydroizolačním souvrství při zkouškách přilnavosti ve smyku
Authors
PLACHÝ, Jan; Jana VYSOKÁ; Radek VEJMELKA; Jan HORSKÝ and Vítězslav VACEK
Edition
1. vyd. Spojené království, IOP Conference Series: Materials Science and Engineering, p. nestránkováno, 7 pp. 2017
Publisher
Institute of Physics Publishing
Other information
Language
English
Type of outcome
Proceedings paper
Field of Study
20101 Civil engineering
Country of publisher
United Kingdom of Great Britain and Northern Ireland
Confidentiality degree
is not subject to a state or trade secret
Publication form
electronic version available online
Marked to be transferred to RIV
Yes
RIV identification code
RIV/75081431:_____/17:00001175
Organization unit
Institute of Technology and Business in České Budějovice
ISSN
Keywords (in Czech)
nízkoviskózní epoxidové pryskyřice;epoxidy; puchýře (boule); primární vrstva; pečetící vrstva; beton; betonová mostovka; izolační system; asfaltový izolační pás; pevnost v tahu; přilnavost ve smyku
Keywords in English
low viscosity epoxy resins;epoxides; blistering (lumps); primary layer; sealing layer; concrete; concrete bridge deck; insulation (waterproofing) system; bitumen (asphalt) waterproofing sheet; tensile strength; shear adhesion
Changed: 20/12/2017 13:15, Mgr. Blanka Mikšíková
In the original language
This paper is based on research dealing with defects that appear on concrete bridge decks with an insulating layer from asphalt strips on the interface between the asphalt strip and its basis. The durability and lifespan of the bearing structure of concrete bridge is determined by insulating layer that constitutes, together with the primary layer and a protective layer, the insulation system of the concrete bridge deck. Paints based on low viscosity epoxy resigns are one of the possibilities of primary layer implementation. These paints may be performed as anchoring-impregnation paints that usually represent single layer paint on the bridge deck surface. Sealing layer is another variant. Sealing layer is a multilayer consisting of anchoring- impregnation paint and sealing paint. The primary layers mainly provide vapour closing of the concrete surface, and partly, through roughening the surface, contribute to adhesion of bitumen (asphalt) insulation (waterproofing) layer. Application of the primary layer has been spreading in the Czech Republic since the 1990s. Now, after approximately 30 years of use defects in these epoxy based sealing layers at the interface between primary layer and waterproofing layer of reinforced bitumen sheets (RBS) are being solved in the Czech Republic. After performance of the first test focusing on breaking-strength, it was found that the strength between the asphalt and the primary belt layer in some types of low-viscosity resin-epoxy decreases and after a certain period of time again increases, depending on the time. Tensile strength test is carried out on a sample of asphalt strip, which is fused onto the substrate with a primer coat. It was therefore proceeded to test the shear adhesion. Testing of the shear adhesion is conducted on the entire concrete deck waterproofing system. It was supposed that the decrease of adhesion at this test become evident in higher extent. Adhesion tests in shear were performed on the primary layer consisting of an anchoring impregnation coating and sealing layer.
In Czech
"Tento příspěvek vychází z výzkumu, který se zabývá problematikou poruch, které se objevují na betonových mostovkách s izolační vrstvou z asfaltových pásů na rozhraní mezi asfaltovým pásem a jeho podkladem. Na životnosti nosné konstrukce betonového mostu se zásadním způsobem podílí izolační vrstva. Izolační vrstva je společně s primární vrstvou a ochrannou vrstvou součástí izolačního systému betonové mostovky. Jedna z materiálových možností provádění primární vrstvy jsou nátěry na bázi nízkoviskózních epoxidových pryskyřic. Tyto nátěry je možné provádět jako kotevně impregnační nátěry, které obvykle představují jednovrstvý nátěr povrchu betonové mostovky. Další variantou je pečetící vrstva. Pečetící vrstva je souvrství, které je tvořené kotevně impregnačním nátěrem a uzavíracím nátěrem. Primární vrstvy, v podobě nátěru, především zvyšují přilnavost izolační vrstvy k podkladu a zajišťují parotěsnost izolačního systému. Rozšíření používání této primární vrstvy je v České republice od 90. let minulého století. Dnes se po cca 20 letech používání řeší v České republice poruchy těchto pečetících vrstev na bázi epoxidů na rozhraní primární vrstva - hydroizolační vrstva z asfaltových izolačních pásů. Po provedení prvních zkoušek, které se soustředily na zkoušku pevnosti v tahu, bylo zjištěno, že u některých typů nízkoviskózních epoxidových pryskyřic dochází v závislosti na čase k poklesu a po určitém časovém období opět k nárůstu pevnosti mezi asfaltovým pásem a primární vrstvou. Zkouška pevnost v tahu je prováděna pouze na vzorku asfaltového pásu, který je nataven na podklad s primární vrstvou. Bylo tedy přistoupeno ke zkouškám přilnavosti ve smyku. U zkoušky přilnavost ve smyku je zkouška prováděna na celém izolačním systému betonové mostovky. Bylo předpokládáno, že projevy poklesu přilnavosti se u této zkoušky projeví ve vyšší míře. Zkoušky přilnavosti ve smyku byly prováděny na primární vrstvě tvořené kotevně impregnačním nátěrem a pečetící vrstvou. "